[MW:6252] Solution Annealing of Stainless Steels

Dear All,
I am slightly confused about solution annealing of stainless steel.
In this process we heat the steel above the temperature range of
sensitisation (upto 900 deg C) and then we suddenly cools it so that
sensitisation temp range passes quickly.

I just want to know does this sudden cooling not increases the
hardness of Stainless Steel.
If No then Why.
If yes then how to avoid that increased Hardness.

Regards,
Mansoor.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...