[MW:6291] API 1104 CODE ISSUE

Dear All,

I need to qualify a welding procedure to API 1104, welding X60 pipe to
Gr. 4130 material. I would like to know if I can do this using a pipe
coupon that is "dual certified X60/X65", or would that pipe only be
usable to qualify an X65 procedure?What consumable I have to use in
this case?

Thanks and Regards


Limesh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...