Modular furnace won't be a problem at all.
regards
On Jul 30, 4:48 pm, suresh venkat <atozsur...@gmail.com> wrote:
> Dear all,
>
> we have several equipments of diameter 5mts & above & length 30 mtrs &
> above. Our specs calls for PWHT in an enclosed furnace.
>
> some of our fabricators expressed inability due to furnace size
> restrictions& informed us that use of Temporary Modular furnaces will pose
> risk to Quality of final product.
>
> I need your advice on the following
>
> 1. Is doing PWHT in modular furnaces will create any problems to the
> equipment (in terms of quality)
> 2. can the temperature be properly controlled
> 3. Pwht can be performed properly without overheating or Under heating.
>
> thanks
>
> Suresh
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment