[MW:6336] PWHT of SA516 gr70 cladded by SS410

Dear All

Can't find this quarry but here is the answer:-

According to UG-40
"When 2 dissimillar P no. metals are welded, like in this case-
PWHT will be done as per UCS66 for the base metal, if PWHT temp. for other material is more then PWHT will be done with the same."



Regards
Manpreet Singh
Welding Engineer
Spiecapag




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...