Saturday, August 7, 2010

[MW:6366] QUENCH& TEMPER


Dear All
we have a steel with approximatly chemical compopsitiuon of: C=.39,CR=.99,,MO=.16& with mechanical properties: yield=321Mpa,UTS=593Mpa,El=29%,A=52%
now we want to quench& temper it to acquire  yield=460-650,maxYs/UTS=.85,min El=18%,average of longitudinal impact=50j
1-does anybody have CCT for this steel?
2-what tempering tempreture is suitable for it to give required toughness property?
regards