[MW:6397] What type of Heat treatment to be done

Dear All

Can anyone suggest me which type of heat treatment to be carried out on a PQR test coupon.  My PQR test coupon is cladded plate Duplex SS UNS S32750 to SA516 Gr.70. Thickness of Duplex SS UNS S32750 is 3 mm and thickness of SA516 Gr.70 is 10 mm. This PQR to be used while welding in two part welded fittings.       

 

Regards

Subrata Das

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...