Dear All,
I have the following qualified WPS as per ASME sec. IX
1) Material Group : P1 (pipe - without backgouging)
Welding process : SMAW
Filler Metal : E 6010 Root run and E 7018 Subsequent run
2) Material group : P1 (plate - with back gouging)
Welding process : FCAW
Filler Metal : E71T
Can I combine these above two WPS to weld Pipe of material SA 106 Gr B root run with SMAW E6010 and subsequent run FCAW E71T .
Thank you with warm Regards,
Manoj