Tuesday, August 10, 2010

[MW:6420] Re: COMBINED WPS & pqr

maybe you need to look back on the table that was provided in ASME
section 9. for more details, please click the link below:
http://frepd.com/2009/04/05/wps-procedures-qualification-1/
and this link :
http://frepd.com/2009/04/05/wps-procedures-qualification-2/

may be helpful
B & R
Achmed

On Aug 10, 10:20 am, manoj john <manojac...@gmail.com> wrote:
> Dear All,
>
> I have the following qualified WPS as per ASME sec. IX
>
> 1)  Material  Group  : P1   (pipe - without backgouging)
>       Welding process  : SMAW
>       Filler Metal         : E 6010 Root run and E 7018 Subsequent run
>
>  2) Material group    : P1 (plate - with back gouging)
>       Welding process  : FCAW
>       Filler Metal          : E71T
>
> Can I combine these above two WPS to weld  Pipe of material SA 106 Gr B root
> run with SMAW  E6010 and subsequent run FCAW E71T .
>
> Thank you with warm Regards,
> Manoj

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...