Friends,
We need to overlay the below material with below recommended electrode or alternative. due to
urgency we cant find in stock. Can any one suggest alternative electrode to achieve same HRC.
Material : SA 240 TY 304 ( 13mm Thick )
Over Lay : 3mm with ( HRC 45 -55)
Recommended Electrode - GRIDUR 65
Classification - DIN 8555-83 - E10-UM-70-GRZ
Regards
D.S.T