Thursday, August 12, 2010

[MW:6452] PWHT for carbon steel piping system working with H2S to perform welding repair

Dear All,

I would like to know about the procedure regarding welding repair in carbon steel piping system that work with products containing H2S. I have received the information that we have to perform three cycles of heat treatment on the test piece used to qualify the welding procedure in order to use this test to perform welding repair on the joints and the number of the cycles means the quantity of repair allowed on the production welds.

Is this procedure correct ? Is this procedured valid only for some groups of materials ? Is there any rule governing this action ? 
 
Could you kindly help me in this query ?

Guttemberg Souza

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...