[MW:6497] RE: 6492] Welder Qualification and reinforcement

Hi,

 

1.As per my view reinforcement is a form of weld deposition where there no fusion with the base metal, so the reinforcement cannot be taken in consideration during the welder qualification, then root penetration is not an variable which is mentioned in the welder qualification, which is left to the designer choice.

 

2.We cannot weld 25 mm plate using 2 welders, as they were qualified to weld 20 mm full welding only, for welding 25 mm plate 1 welder qualified up to 20 mm can be used whereas the 2nd welder must be qualified for welding the repair welding.

 

Regards,

Prasanna.R.U.

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ather .
Sent: 14 August 2010 13:35
To: materials-welding@googlegroups.com
Subject: [MW:6492] Welder Qualification and reinforcement

 

Hi Guys,

 

1) I wonder why we will not consider the reinforcement and Root penetration in welder qualification thickness range..? as this is also a form of weld deposition.

 

2) Can we weld a 25 mm thick plate using 2 welders each is qualified to weld 20mm.Welding code is AWS D 1.1

 

Hope to have your helpful answers.

 

Thanks & Regards,

Ather

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

__________ Information from ESET NOD32 Antivirus, version of virus signature database 5365 (20100813) __________

 

The message was checked by ESET NOD32 Antivirus.

 

http://www.eset.com



__________ Information from ESET NOD32 Antivirus, version of virus signature database 5367 (20100814) __________

The message was checked by ESET NOD32 Antivirus.

http://www.eset.com

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...