 what is the purpose of using a dual certified material.
 
 
 Example -  Plate  used for vessel fabrication as per ASME SEC VIII DIV1 is  dual certified as SA 516 GR 60 and SA 516GR70.
 
What will be the tensile strength of this plate and impact properties. whether these properties will be as per SA516 GR 60  OR sa 516 GR. 70.
 
Thanks in Advance.
 
Regards
 
Asad

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...