[MW:6518] How to manufacture Welded Stub End

Dear All,
Please guide me how to manufacture welded stub end. In ASTM A403, 2004
edition it was allowed to weld the lap on pipe but in 2007 that clause
is been deleted.
Can we expand the welded pipe to form a lap?
Please Help!
Regards