[MW:6549] Conflict about heat available on electrode/work for the SMAW & GTAW process even having same polarity

Dear all,


1. For SMAW-DCEN-2/3 heat to the electrode.
2. For GTAW-DCEN-2/3 heat to the work.

Why this is conflict?
Theoretically more heat is produced where the bombardment of electrons
is carried out.
Please give me clarification justification with proper evidence.

Regards,
Maulik H. Thakkar
Welding engineer

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.