[MW:6615] Simulation of Carbon Steel Dished End Normalised After Forming

Dear All,

I have Carbon Steel Dished End in which Normalising is required after
forming as per customer specifications.The thickness is 28mm due to
hydrogen service PWHT is required for 60minutes.

My Questions:

1. As the material is carbon steel and simulation is required as per
UCS 85(f), because my material is going above lower transformation
temperature. What should be the simulation cycle?

Do i need to give the SR cycle in simulation? i mean simulation of N
+SR

2. and if i have the simulation available N+SR, and i need to Re SR
the job due to shop repair. Do i need the simulation N+SR+SR or the
simulation available above is OK.

Regards

Jaspal Singh
ISGEC-Yamunanagar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...