[MW:6623] Manufacturer PQR Test results of 25 Cr 35 Ni to SA 479 TYP 304H - furnace tubes

Hi,

 

Manufacturer PQR Test results of 25 Cr 35 Ni to SA 479 TYP 304H - furnace tubes

 

Tensile test of the 13 mm thick specimen results in 2.67 % & 3.7 % elongation

 

Bend test (As per ASME IX) failed at the HAZ. Manufacturer has followed ASTM A 488 "Standard specifications for steel castings, Welding, Qualification of procedures and personnel" to qualify the procedure.

 

Question

 

1.       Is the PQR qualified if QW-466.19 [General notes (E)] is followed?.

 

"QW-466.19 - For material with less than 3 % elongation, a macro etch specimen shall be used in lieu of bend test at each bend location. Acceptance criteria shall be in accordance with QW-183(a)".

 

2.       Can ASTM A 488-8.2.4 be followed to qualify a procedure?

 

"ASTM A 488-8.2.4 – Where the ductility of the parent metal is such as to render it incapable of meeting the bend test requirements, the bend test shall be conducted in the following manner: A bend bar comprised of parent metal heat treated to the ductility & strength requirements of the applicable specifications shall be bent to failure. The side bend specimen shall be then capable of being bent to within 5° of the angle thus determined."

 

Regards,

kareem


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...