[MW:6635] RE: 6634] Paint Consumption

Surface area x DFT x S
 
"S" is a spill factor - typical approximately 2. Covering what does not hit the steel surface and that what exceeds the pot life time.
 
But note: For calculating man-hour consumption for a painting job, the preparation (sand blasting, etc.) is the dominant factor.
 
regards
Kristian 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ramesh Barot
Sent: 23. august 2010 07:16
To: Materials Welding
Subject: [MW:6634] Paint Consumption

Dear All,
 
Can anybody guide me how can we calculate the paint consumption on steel?
 
Thanks in Advance,
With Best Regards,
Ramesh Barot

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.