Guys,

In accordance with ASME IX QW461 positions.

If I test welders on plate and tilt the joint to 80 degrees does that mean on one test butt weld I can qualify my welders for 3G and 4G?

Comments please.

 

William Lusk

Senior Welding Engineer

Tel. : +966(4)3961171

Ext. : 344

Mobile+966 55 880 0431

E-mail : william.lusk@yanbusteel.com

billlusk66@yahoo.com

 



This e-mail and any files transmitted with it are confidential and intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the system manager. Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of the company. Finally, the recipient should check this e-mail and any attachments for the presence of viruses. The company accepts no liability for any damage caused by any virus transmitted by this e-mail.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point