Please refer to NACE MR 0175 / ISO 15156.
The partial pressure (mole concentrafion of H2S times the line pressure) of H2S decides and there are more regimes, shown in curves in NACE MR 0175 / ISO 15156. At relative small line pressures, 50 ppm will not result in sour service conditions.
regards
Kristian


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Manav Malhotra
Sent: 24. august 2010 17:35
To: materials-welding@googlegroups.com
Subject: [MW:6686] Sour Service

Dear Members,
 
Can anyone clarify whats the requirment of sour service. Some say presence of H2S or if H2S is more than 50 ppm.
 
Regards,
Manav Malhotra

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...