Hi,

 

You require new PQR for welding P8 to P8.

 

Prasanna.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of William Lusk
Sent: 25 August 2010 10:40
To: materials-welding@googlegroups.com
Subject: [MW:6699] RE: 6694] PQR Validity

 

Sandeep,

The welder is qualified to weld s/s P8 using the GTAW because it is the same F No 6 .

The welder is not qualified for SMAW because the FNo are different C/S F No 4 E7018 the S/S is FNo 5 so he would need to be tested for SMAW welding.

YOU will need a PQR qualified for the S/S material as it is an essential variable but welders as stated above are OK.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Chan, David
Sent: Wednesday, August 25, 2010 6:51 AM
To: materials-welding@googlegroups.com
Subject: **** SPAM **** [MW:6695] 6694] PQR Validity

 

Sandeep,

Please refer to ASME IX for a better understanding as the welder is NOT qualified to weld P8 based on P1

 

You will require a new PQR for P8

 

Thank you,

 

Best Regards.

 

David Chan


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of sandeep
Sent: Wednesday, August 25, 2010 2:11 AM
To: materials-welding@googlegroups.com
Subject: [MW:6694] PQR Validity

 

Hello Everybody

 I have qualified (2005) GTAW     PQR#1 for  Material of  (P1 Gr 2) to ( P1 Gr 2).
I have WPS #1 for the same.

Welders qualify for WPS#1
I have question

1.If I want Welder to weld  Material Of P8 Gr 1
I have to develop new PQR ?
 

If you need more info let me know

Thanks

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


This e-mail and any files transmitted with it are confidential and intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the system manager. Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of the company. Finally, the recipient should check this e-mail and any attachments for the presence of viruses. The company accepts no liability for any damage caused by any virus transmitted by this e-mail.

 


This e-mail and any files transmitted with it are confidential and intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the system manager. Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of the company. Finally, the recipient should check this e-mail and any attachments for the presence of viruses. The company accepts no liability for any damage caused by any virus transmitted by this e-mail.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

__________ Information from ESET NOD32 Antivirus, version of virus signature database 5394 (20100824) __________

 

The message was checked by ESET NOD32 Antivirus.

 

http://www.eset.com



__________ Information from ESET NOD32 Antivirus, version of virus signature database 5394 (20100824) __________

The message was checked by ESET NOD32 Antivirus.

http://www.eset.com



__________ Information from ESET NOD32 Antivirus, version of virus signature database 5394 (20100824) __________

The message was checked by ESET NOD32 Antivirus.

http://www.eset.com



__________ Information from ESET NOD32 Antivirus, version of virus signature database 5394 (20100824) __________

The message was checked by ESET NOD32 Antivirus.

http://www.eset.com



__________ Information from ESET NOD32 Antivirus, version of virus signature database 5394 (20100824) __________

The message was checked by ESET NOD32 Antivirus.

http://www.eset.com

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...