[MW:6705] Re: How to protect Serration of Flanges during Hot dip galvanization

Molykote 1000 of Dow Corning Product will withstand upto 650 deg C,
anyway you can apply that uniformly and do hot dipping; but ensure no
removal of the coating while dipping.


On Aug 23, 1:38 pm, aly mhaskar <mhaskar_...@yahoo.com> wrote:
> Dear All,
> Presently we are doing hot dip galvanization of pipe spools where we have to
> protect the serration of flanges during galvanization.
>
> Can any body suggest what can be applied on serration to protect it
> from adhesion of ZINC on serration.
>
> Thank you in advance.
>
> Mhaskar Aly
> Kuwait

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...