[MW:6707] Reg Range of Amperage in WPS

Dear All,

Can any one help me!

PQR Qualified with an amperage of min 350 and max 550.
As per AWS D1.1, Allowable Variation in Amperage for WPS is 10 %.
How should i consider this 10%.

Case 1
Should i Consider lesser 10 % lesser to PQR's Min Amperage and
Greater side 10 % to the max PQR Amperage.

Case 2
Or Should i consider 10% min max of Average of PQR Value.

Which case is correct?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...