It is not the conflict.
Pls understand the difference between the Thermionic & Non-Thermionic
cathodes,
That will explains the heat distribution. Pls go through the topic of Arc
Physics in ASM Welding Handbooks
Rgds,
K.Babu
Singapore
----- Original Message -----
From: "MAULIK" <mlkthakkar2@gmail.com>
To: "Materials & Welding" <materials-welding@googlegroups.com>
Cc: <bhavesh.patel@isgec.com>
Sent: Wednesday, August 18, 2010 1:47 AM
Subject: [MW:6549] Conflict about heat available on electrode/work for the
SMAW & GTAW process even having same polarity
> Dear all,
>
>
> 1. For SMAW-DCEN-2/3 heat to the electrode.
> 2. For GTAW-DCEN-2/3 heat to the work.
>
> Why this is conflict?
> Theoretically more heat is produced where the bombardment of electrons
> is carried out.
> Please give me clarification justification with proper evidence.
>
> Regards,
> Maulik H. Thakkar
> Welding engineer
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment