For welding 6 mm with GTAW you have to make single V with root gap at least 3mm.and with just two-three passes you can fill up 6mm of grove. Before applying SAW you shall have atleast 5-7 mm of weld metal as back up to avoid burn through So in this case no point in using SAW.

However if you want to use SAW to increase productivity, its better to go with Square butt with 0 (no) gap. I have tried this practically and achieved sound weld (RT without any defects) with good penetration.

Regards.

On 31 July 2010 14:37, Eng/ Mostafa Kamel Hussein <mkh_200@yahoo.com> wrote:
What is the suitable joint design (single V, square, bevel, ........)  for plate SA-283 Gr.B (S235JR) as the thickness is 6mm and the processes used is GMAW/FCAW+SAW

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
C. K. Purohit
Eng-Tech Weld1
Sr Welding Inspector

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...