Re: [MW:6236] why plsama cutting in ss

when u are heating, oxides forms. Oxy-acet has a Kindling temp of 1200 celcius. If any oxides after haeting exceeds this temp can not be cut by oxy-ace flamme
KGP

On Tue, Jul 27, 2010 at 7:10 PM, mijin <mathew.mijin@gmail.com> wrote:
why we are using plasma cutting in stainless steel instead of
oxyacetelene cuttng.please give me a reason...

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...