Sunday, August 1, 2010

RE: [MW:6237] minimum butt weld joint

 

Dear Saha

 

Thnx for your helpful below mail, actually, I was asking for such code having such regulations, if there is or not.

Since I had never face the same –butt weld less than 2”-, & I read it before in Shell DEP standards, so I was thinking it is applicable for BS & ASME codes also.

 

Thanx again

 

Rgrads

Majdi

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of saha ja
Sent: Sunday, August 01, 2010 7:30 AM
To: materials-welding@googlegroups.com
Subject: RE: [MW:0] minimum butt weld joint

 

Hi,

 

Find some Information which can help regarding selection of Butt and Socket.



When do you NOT want to use socket-welded fittings?

- in severely vibrational services as others have said

- in severely corrosive or high purity services, because all socket-welded fittings contain a deep crevice ideal for corrosion

- for high toxicity services where a radiographic inspection of each weld's integrity is required

- where the flexibility analysis tells you that they're no good because of the stress intensification issues indicated above (a rarety if the piping is otherwise designed and supported correctly)

- in services with expensive materials of construction (i.e. titanium etc.), because the extra material required in the SW versus BW fittings will often eat any savings in welding cost (combined with the corrosion issue above!)

- any time your welders are not familliar enough with them to realize that they must be fit with a shrinkage gap- it's the fittings which have been bottomed in the socket before welding that are most prone to failure

- beyond about 3" pipesize, regardless

When do you WANT to use socket-welded fittings?  Virtually in all other circumstances where threaded connections have been ruled out.  Socket-welded piping is quicker and easier to both fit AND weld and hence is far less expensive than the butt-welded alternative.  Savings of 50%+ in installed cost can be expected in practice relative to butt welding.

Clearly your results may vary, but that's my take on the issue.  Be careful about axiomatic statements, whether from me or others, that you might hear on this site!  Case in point: unclesyd's "RTJ flanges are used on all heating fluid services".  Although I bow at unclesyd's feet as he is an extremely knowledgeable engineer and I listen carefully to what he says, there are plenty of places where ordinary raised-face gasketed ANSI flanges are perfectly fine for use with heating fluids.  Even 150# flanges, though I know there are people and companies which just say no to them for hot oil...

Regards,

SAHA


From: melyyan@gmail.com
To: materials-welding@googlegroups.com
Subject: [MW:6222] minimum butt weld joint
Date: Sat, 31 Jul 2010 19:05:10 +0400

Dear all;

 

I had a question regarding minimum butt weld joint?

 

Is there any code mentioning that NPS 2 & above shall be butt weld joints & less than 2” socket weld?

 

Please advice?

 

Regards

Majdi


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...