Re: [MW:6243] How to select the IQI wire

Venkat,
 
Which IQI? ASTM, DIN(ISO), FE EN? all differes and depends upon thickness of the object being radiographed...Diameter is not  a concern.
 
regards,
Nandeesh

--- On Mon, 2/8/10, venkat ramana <venkatgps.ramana@gmail.com> wrote:

From: venkat ramana <venkatgps.ramana@gmail.com>
Subject: [MW:6239] How to select the IQI wire
To: materials-welding@googlegroups.com
Date: Monday, 2 August, 2010, 4:48 AM

Dear All,
 
let me know how to select the IQI wire of carbon steel 6inch sch 80 reference code is B31.3 material as P1 please reply me as soon as possible.
 
Thanks & Regards
venkat (QC)
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...