Monday, August 2, 2010

RE: [MW:6244] How to select the IQI wire

Dear Venkat

 

Applicable test standards: ASME Sect. V Art.2 for procedure, Pipe 6” SCH80, norm. Thk 11.0. Exp. Technical: DWSI, IQI on film side, essential wire number 6 (dia. 0.25) So you can select ASTM 1A 6 or ASTM 1B 11.

 

 

Best regards

 

TRAN VAN VUONG

Email: vuongtv@phateco.com


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Nandesh Kumar
Sent: Monday, August 02, 2010 2:26 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:6243] How to select the IQI wire

 

Venkat,

 

Which IQI? ASTM, DIN(ISO), FE EN? all differes and depends upon thickness of the object being radiographed...Diameter is not  a concern.

 

regards,

Nandeesh

--- On Mon, 2/8/10, venkat ramana <venkatgps.ramana@gmail.com> wrote:


From: venkat ramana <venkatgps.ramana@gmail.com>
Subject: [MW:6239] How to select the IQI wire
To: materials-welding@googlegroups.com
Date: Monday, 2 August, 2010, 4:48 AM

Dear All,

 

let me know how to select the IQI wire of carbon steel 6inch sch 80 reference code is B31.3 material as P1 please reply me as soon as possible.

 

Thanks & Regards

venkat (QC)

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...