Monday, August 2, 2010

Re: [MW:6246] Painting Service Plan?

Mohan :

To my knowledge Painting Service Plan is documented procedure on how painting service will be done and how to assure that painting service you provide will met Client Requirements.

It is like a document that from this Clients could measure your level of knowledge and readiness to handle the job.

The documents covers coating materials, coating test protocol and acceptance criteria, surface preparation, coating application, quality assurance and control, and repair methods.

Regards

Richard Napitupulu
QA/QC Engineer
PHE-ONWJ

From: redbull <mohanq8@gmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Sat, 31 July, 2010 2:00:14 PM
Subject: [MW:6215] Painting Service Plan?

Dear Folks,

Can some one clarify what is Painting Service Plan for Off-Shore
(above water)  Painting Maintenance contract. If some one has sample
for model Plan please share.



--
With Regards,

Mohan, Q8.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...