Re: [MW:6260] How to select the IQI wire

This for sample, 6" sch 80 is 0.432 in (10.973 mm) if Low pressure it would be 13.973mm thickness + reinforcement included, use ASTM 1B or 10 FE EN
 
Make sure ASTM or EN or what kind IQI mentioned in RT procedure.
 
 
Leo Sudarmadji
RT Supv.
NDTS

--- On Mon, 8/2/10, george.dilintas@gr.bureauveritas.com <george.dilintas@gr.bureauveritas.com> wrote:

From: george.dilintas@gr.bureauveritas.com <george.dilintas@gr.bureauveritas.com>
Subject: Re: [MW:6254] How to select the IQI wire
To: "materials-welding" <materials-welding@googlegroups.com>
Date: Monday, August 2, 2010, 8:33 PM

Sorry but you should refer to T276.2(a) of section V

  From: "Tran Van Vuong" [vuong.tv@gmail.com]
  Sent: 02/08/2010 16:03 ZE7
  To: <materials-welding@googlegroups.com>
  Subject: RE: [MW:6248] How to select the IQI wire

Dear Venkat

Thickness of weld does not include any reinforcement as ASME specified.

 

Best regards

 

TRAN VAN VUONG

Email: vuongtv@phateco.com


From: materials-welding@googlegroups.com [mailto: materials-welding@googlegroups.com ] On Behalf Of tong tong
Sent: Monday, August 02, 2010 3:41 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:6245] How to select the IQI wire

 

 

Don't forget to add reinformence cap height in order to get the material thickness range

Regards 

On Mon, Aug 2, 2010 at 3:54 PM, Tran Van Vuong <vuong.tv@gmail.com> wrote:

Dear Venkat

 

Applicable test standards: ASME Sect. V Art.2 for procedure, Pipe 6" SCH80, norm. Thk 11.0. Exp. Technical: DWSI, IQI on film side, essential wire number 6 (dia. 0.25) So you can select ASTM 1A 6 or ASTM 1B 11.

 

 

Best regards
 
TRAN VAN VUONG

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Nandesh Kumar
Sent: Monday, August 02, 2010 2:26 PM

Subject: Re: [MW:6243] How to select the IQI wire

 

Venkat,

 

Which IQI? ASTM, DIN(ISO), FE EN? all differes and depends upon thickness of the object being radiographed...Diameter is not  a concern.

 

regards,

Nandeesh

--- On Mon, 2/8/10, venkat ramana <venkatgps.ramana@gmail.com> wrote:


From: venkat ramana <venkatgps.ramana@gmail.com>
Subject: [MW:6239] How to select the IQI wire
To: materials-welding@googlegroups.com
Date: Monday, 2 August, 2010, 4:48 AM

Dear All,

 

let me know how to select the IQI wire of carbon steel 6inch sch 80 reference code is B31.3 material as P1 please reply me as soon as possible.

 

Thanks & Regards

venkat (QC)

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...