Re: [MW:6290] WPS for API 5L X Grades

Dear Mr.Bathulla,
 
The below mentioned WPS qualified for the CODE API 1104, B 31.4 and B 31.8, at present I am going to use the mentioned material for code B 31.8.


On Tue, Aug 3, 2010 at 2:49 PM, murali krishnan <muraligkrishnan@gmail.com> wrote:
Dear Mr.Bathulla,
 
The below mentioned WPS qualified for the CODE API 1104, B 31.4 and B 31.8.

On Tue, Aug 3, 2010 at 2:39 PM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:
What is your code of construction?

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of murali krishnan
Sent: Tuesday, August 03, 2010 5:03 PM
To: materials-welding@googlegroups.com
Subject: [MW:6287] WPS

Dear All,
 
We have a WPS qualified for API 5L Gr X -65 to API -5L Gr X42,X52,X60/X65, of diameter range above 12 3/4" with wall thickness 3/16" - 3/4", welding done with SMAW process, electrode used for root is  E 7010P1 and rest with E 8018C3, "My query is whether we shall do the welding with same WPS for API 5L Gr X 60  to API 5L Gr X 60 if not we have to prepare new WPS for the mentioned material.

G.Murali krishnan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
G.Murali krishnan



--
G.Murali krishnan
QA/QC Supervisor
Saudi Arabian Saipem Ltd.
MGS UBTG 4 Extension & BJBFG 3 P/L
Saudi Arabia
+966-552000114
+966-548161675

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...