Dear ALL,
 
You don't need to prepare new WPS as long as the pipe material is the same ( API 5L ).
 
THIS IS In accordance with ASME SEC IX / QW 403.
 
Regards,
 
Sohaib Ghnaimat

--- On Tue, 8/3/10, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:

From: Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com>
Subject: [MW:6288] WPS for API 5L X Grades
To: "'materials-welding@googlegroups.com'" <materials-welding@googlegroups.com>
Date: Tuesday, August 3, 2010, 2:39 PM

What is your code of construction?

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of murali krishnan
Sent: Tuesday, August 03, 2010 5:03 PM
To: materials-welding@googlegroups.com
Subject: [MW:6287] WPS

Dear All,
 
We have a WPS qualified for API 5L Gr X -65 to API -5L Gr X42,X52,X60/X65, of diameter range above 12 3/4" with wall thickness 3/16" - 3/4", welding done with SMAW process, electrode used for root is  E 7010P1 and rest with E 8018C3, "My query is whether we shall do the welding with same WPS for API 5L Gr X 60  to API 5L Gr X 60 if not we have to prepare new WPS for the mentioned material.

G.Murali krishnan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...