Wednesday, August 4, 2010

RE: [MW:6300] formula for calculating elongation

Is it for the forming strain? In ASME Sec VIII div 1, you can use the formula given UHA 44 or UNF79

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of boris ochije
Sent: Tuesday, August 03, 2010 8:13 PM
To: materials-welding@googlegroups.com
Subject: [MW:6294] formula for calculating elongation

sir pls what is the formula for calculating elongation in duplex pipes and carbon steel plates and pipes.

from boris ochije



Filtered by Hosted Filtering


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...