1. NB-23 is a post construction CODE while PCC-2 is a STANDARD.
2. NB-23 defines administrative and technical requirements needed to inspect, repair or alter pressure retaining parts while PCC-2 only provides technical methods for repair of equipments & piping.
3. NB-23 is not limited to any specific construction code/standard while PCC-2 only covers ASME construction codes/standards
4. NB-23 only deals with permanent nature of repairs while PCC-2 deals with both natures of repairs (temporary + permanent).


--
Welder's Helper
 
Never bend my head infront of anyone other than GOD the almighty.


On Tue, Aug 3, 2010 at 6:43 PM, limesh M <limesh78@gmail.com> wrote:
Dear All,

What is the scope of NBIC NB-23? Comparison with ASME PCC-2?

Taking an example of a pressure vessel thickness loss in bottom dish
end, how would NBIC NB-23 would deal that in comparison to PCC-2?


Thanks and Regards,


Limesh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...