Dear Mr. Shukri
What is the construction code?
To decide whether Impact testing shall be performed on a material, you should ist decide MDMT.
UG-20 requires the MDMT to be established for the lowest operating temperature, operational upsets,auto-refrigeration, atmospheric temperature, or any other sources of cooling.
Once you decide MDMT, Refer UHA-51 to decide whether impact testing is applicable or not?
Regards
Manpreet Singh
Welding Engineer
Spiecapag
On Sat, 07 Aug 2010 08:50:44 +0530 wrote
>Hi all,
I have one query about the charpy impact test. Do the stainless steel (P-No.8), Duplex & Super Duplex (P-No.10H) required charpy impact test or not? If yes, what condition which I need to consider when doing the charpy impact test and where can I refer?
Thank you,
Regards,
Shukri
--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment