Re: [MW:6367] Re: DOLLYMIX WELDING

Dear All,
 
Could you please give some literature explaining the term 'DOLLYMIX'.
 
Regards,
 
Limesh
 


 
On Sat, Aug 7, 2010 at 12:46 PM, sumit jaura <sumit.jaura@gmail.com> wrote:
Dear Limesh,,


It is called dolly mix because first pass is uphill and remaining pass
are downhill,

moslty qualified as WPS-02. Dollymix is often has more strength than
downhill welding.



On Aug 6, 11:22 am, limesh M <limes...@gmail.com> wrote:
> Dear All,
>
> Is there any technical term called 'Dollymix' in pipeline welding?
>
> I searched lot of literature but all efforts are in vein.I found that
> many contractors WPS says 'Dollymix' progression !!!
>
> Root pass uphill and remaining downhill called dollymix or root and
> hot pass uphill and remaining downhill called dollymix? Is it a local
> terminology or worldwide accepted one?
>
> Regards,
>
> Limesh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...