Are we sure there is no catch here- The certification of supplier by his independent QA/ QC department.....? I think it has to be an independent 3rd party lab or similar.
--- On Sat, 7/8/10, JASPAL SINGH <jaspaldhesi@gmail.com> wrote:
From: JASPAL SINGH <jaspaldhesi@gmail.com> Subject: [MW:0] Re: BS EN-10204 3.1 & 3.2 To: "Materials & Welding" <materials-welding@googlegroups.com> Date: Saturday, 7 August, 2010, 3:46 PM
BS EN-10204 3.1: The certification of supplier by his independent QA/ QC department. Where as 3.2 is Witness of Testing required as per Technical Delivery Conditions. Regards Jaspal Singh, CWI-AWS, CSWIP-3.1 Assistant Manager – Quality Assurance Process Equipment Division ISGEC, Yamuna Nagar, Haryana -135001 Phone: 911732307251 Ext: 251 Mb: +918930111441 "To love what you do and feel that it matters - how could anything be more fun?" On Aug 7, 2:31 pm, Noushad cp < ncp....@gmail.com> wrote: > Dear All, > > I would like to know the diffrence between 3.1 and 3.2 Certification. > > Please explain in detail way.Applicable test and all. > > Regards, > > NCPTesting -- To post to this group, send email to materials-welding@googlegroups.comTo unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.comFor more options, visit this group's bolg at http://materials-welding.blogspot.com/The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
|
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.