Dear Senthil,

Being glad to contact you, i am herewith suggesting you to go with the Hardfacing electrode which will conform to DIN-8555 E10-UM-65-GRZ. Since we are dealing Bohler
welding Group electrodes [Bohler (Austria), UTP(Germany)], the recommended brand
for your specification is UTP LEDURIT 65.

Moreover, if you give some more details about the application (like Industry type/Equipment /Working medium/Wear type/Impact or Temperature involved, Static or Dynamic ), it will be always better to select the suitable hardfacing electrode. As you know well, the selection of Hardfacing electrodes will depend on many factors.

Anyhow, i have attached the catalogue of UTP Brand electrode for your evaluation. Definitely it will give very good results in wear resistance/service life compared to Lincoln's Gridur 65.

If you tell your job location, i will inform you from where you can get the above said.

Thanks and Regards,

M.SarojKumar
Sales Manager-Welding Products
Alruqee Industrial Marketing Co Ltd,
Saudi Arabia.
Mobile: +966 5662 05444 


On Wed, Aug 11, 2010 at 10:20 AM, greetings <senthilthandesh@gmail.com> wrote:
Friends,
 
We need to overlay the below material with below recommended electrode or alternative. due to
urgency we cant find in stock.  Can any one suggest  alternative electrode to achieve same HRC.
 
Material : SA 240 TY 304 ( 13mm Thick )
Over Lay : 3mm with ( HRC 45 -55)
 
Recommended Electrode - GRIDUR 65
Classification - DIN 8555-83 - E10-UM-70-GRZ
 
 
Regards
D.S.T
 
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...