No, qualified to weld pipe out side diameter 73mm and above (QW452.3).
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of venkat ramana
Sent: Thursday, August 12, 2010 12:29 PM
To: materials-welding@googlegroups.com
Subject: [MW:6454] Welder qualification
Dear All,
Please let me know with reference, query is A welder has been tested in the 6-G position, using as E-7018 F-4 electrode, on 6inch sch160 SA106B pipe. Is this welder qualified to weld a 2ich 300# ANSI sch80 bore flange to a 2inch sch80 SA106B nozzle neck?
Thanks Regards
Venkat (QA/QC Inspector, Qatar)