Thursday, August 12, 2010

Re: [MW:6468] Welder qualified

No.

F-No. of both E7018 and E8028 is different.

Regards,

Ashfaq

thepetrostreet.com

On Thu, 12 Aug 2010 13:53:57 +0300, venkat ramana <venkatgps.ramana@gmail.com> wrote:

Dear All,
 
Please let me know, my query is A welder was qualified with a P-1 test coupon using SMAW E7018 electrodes. May the welder weld P-4 material using E8028 electrodes with backing in production? (Assume the P-4 procedure using E8028 electrodes has been qualified)
 
Thanks & Regards
Venkat
 
 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...