Yes if all other parameters fit
From: venkat ramana [venkatgps.ramana@gmail.com]
Sent: 12/08/2010 13:53 ZE3
To: materials-welding@googlegroups.com
Subject: [MW:6466] Welder qualified
Dear All,
Please let me know, my query is A welder was qualified with a P-1 test coupon using SMAW E7018 electrodes. May the welder weld P-4 material using E8028 electrodes with backing in production? (Assume the P-4 procedure using E8028 electrodes has been qualified)
Thanks & Regards
Venkat
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment