Re: [MW:6475] P42 (Monel) to P1 (SA516 G.70) Welding

U can butter the cs then pwht the buttered and then weld the nozzle without pwht


  From: Muhammed Ibrahim PK [ibratech@gmail.com]
  Sent: 12/08/2010 12:13 ZE4
  To: materials-welding@googlegroups.com
  Subject: [MW:6458] P42 (Monel) to P1 (SA516 G.70) Welding


Gents,
 
We have to weld a monel Nozzle SB165 (UNS N04400) (P No.42) to SA516G.70 (PNo.1) 45 mm thk
 
The vessel is required PWHT.
 
I need to qualify a PQR for this welding with ERNiCu+ENiCu-7.
 
Is it required to do PWHT of this joint (P42 to P1)?.
 
If PWHT is required what is the way of  welding of this joint?
 
If  PWHT is not required what is the procedure to weld it?
 
Is it required to butter the CS with monel before butt welding?
 
Is any post heting is required for this joint?
 

Thanks & Regards
Muhammed Ibrahim PK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...