Hi,

Yes, he can weld with backing. Refer QW 433 table.

Thanks & Regards
Muhammed Ibrahim PK



On 13 August 2010 14:46, Balaji <balaji.weldingeng@gmail.com> wrote:
Dear Venkat
                 Nope. He can't weld P-4 material using
E8028 electrodes, since F numbers are different. As per Sex IX, for
welder qualification, F numbers are essential variables.


Regards

Balaji
On Aug 12, 2:53 pm, venkat ramana <venkatgps.ram...@gmail.com> wrote:
> Dear All,
>
> Please let me know, my query is A welder was qualified with a P-1 test
> coupon using SMAW E7018 electrodes. May the welder weld P-4 material using
> E8028 electrodes with backing in production? (Assume the P-4 procedure using
> E8028 electrodes has been qualified)
>
> Thanks & Regards
> Venkat

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...