As P-Number is an essentially variable, when the welder qualified with the P-1 WPS,PQR cannot be used for the P-4 material, hence requalification if required. It is for your kind attention QW 433 describes about F-No. only not about the P number.

 

Regards,

Prasanna.R.U.

Bureau Veritas,Chennai

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Muhammed Ibrahim PK
Sent: 13 August 2010 17:26
To: materials-welding@googlegroups.com
Subject: Re: [MW:6482] Re: Welder qualified

 

Hi,

 

Yes, he can weld with backing. Refer QW 433 table.


Thanks & Regards
Muhammed Ibrahim PK


On 13 August 2010 14:46, Balaji <balaji.weldingeng@gmail.com> wrote:

Dear Venkat
                 Nope. He can't weld P-4 material using
E8028 electrodes, since F numbers are different. As per Sex IX, for
welder qualification, F numbers are essential variables.


Regards

Balaji
On Aug 12, 2:53 pm, venkat ramana <venkatgps.ram...@gmail.com> wrote:
> Dear All,
>
> Please let me know, my query is A welder was qualified with a P-1 test
> coupon using SMAW E7018 electrodes. May the welder weld P-4 material using
> E8028 electrodes with backing in production? (Assume the P-4 procedure using
> E8028 electrodes has been qualified)
>
> Thanks & Regards
> Venkat

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

__________ Information from ESET NOD32 Antivirus, version of virus signature database 5361 (20100812) __________

 

The message was checked by ESET NOD32 Antivirus.

 

http://www.eset.com

 

__________ Information from ESET NOD32 Antivirus, version of virus signature database 5365 (20100813) __________

 

The message was checked by ESET NOD32 Antivirus.

 

http://www.eset.com



__________ Information from ESET NOD32 Antivirus, version of virus signature database 5365 (20100813) __________

The message was checked by ESET NOD32 Antivirus.

http://www.eset.com

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...