Hi,

The welder can weld using both E7018 and E8018 since F number are same.Pls.Refer QW432 (E7018 - SFA5.1-F.No.4 and E8018-SFA5.5-F.No.4)


Karthikeyan.S
 
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Fri, 8/13/10, Balaji <balaji.weldingeng@gmail.com> wrote:

From: Balaji <balaji.weldingeng@gmail.com>
Subject: [MW:6479] Re: Welder qualified
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Friday, August 13, 2010, 5:46 PM

Dear Venkat
                  Nope. He can't weld P-4 material using
E8028 electrodes, since F numbers are different. As per Sex IX, for
welder qualification, F numbers are essential variables.


Regards

Balaji
On Aug 12, 2:53 pm, venkat ramana <venkatgps.ram...@gmail.com> wrote:
> Dear All,
>
> Please let me know, my query is A welder was qualified with a P-1 test
> coupon using SMAW E7018 electrodes. May the welder weld P-4 material using
> E8028 electrodes with backing in production? (Assume the P-4 procedure using
> E8028 electrodes has been qualified)
>
> Thanks & Regards
> Venkat

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...