Saturday, August 14, 2010

Re: [MW:6491] what is formula of miter cut elbow?

hi,
please refer ASME B31.1 section 104.3.3 and Mandatory Appendix-D..you can find all detail formula for miter elbows.
 
Thanks & Regards,
 
(Karthik)

Karthikeyan.S
 
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Sat, 8/14/10, Usman Anwar <usmananwarlhrpk@gmail.com> wrote:

From: Usman Anwar <usmananwarlhrpk@gmail.com>
Subject: [MW:6490] what is formula of miter cut elbow?
To: materials-welding@googlegroups.com
Date: Saturday, August 14, 2010, 11:24 AM

dear friends,
i want to know abt the formula for miter cut elbow of dia 24 inch?thanks
regards
usman

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...