Dear Mr.Khan,
 
To minimise the Heat Input,we are using Dollymix welding Technique.
 
Thanks.
 
Piramaryan B
Welding Engineer -CSWIP SCWI 3.2.2
ILF CONSULING ENGIEERS (PMC) KSA

 
On Wed, Aug 11, 2010 at 8:41 PM, aslam khan <aslamkhan4u@gmail.com> wrote:
dear all ,
i want to know  why do we use dollymix welding technique in pipelines?thanks

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...