Tuesday, August 17, 2010

RE: [MW:6530] simulation treatment

Pl. refer UCS 85


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Muhammed Ibrahim PK
Sent: Tuesday, August 17, 2010 9:16 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:6529] simulation treatment

Hi,
 
Simulation heat treatment is performing on sample piece of material to be used in production.
If the production required PWHT for 2 Hrs, do PWHT in the sample piece of the material for three cycle. ie 6hrs. then carry out the tensile test and hardness test & if applicable impact also.
 
If any production repair required we have to confirm the property of material is safe after multiple PWHT.

Thanks & Regards
Muhammed Ibrahim PK


On 16 August 2010 23:06, asad azmi <azmiasadayub@gmail.com> wrote:
Dear All,
 
Greetings.
 
what is simulation  Treatment and where it is applicable.
 
 Please  expalin with example in reference to ASME SEC VIII DIV 1/ASME SEC II
 
Thanks in advance.
 
Regards
 
Asad 


No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...