Dual certificate menas
 
Chemical properties compliance with of lower grade material i.e Gr 60 & mechanical properties  compliance with higher grade materials i.e of Gr.70

Customer has specific requirments particular chemical & mechanical properties thts why they specify dual grade material or certificate required.
 
Hope the matter is useful.
 
Regards,
Vikas Rana
 
 
On Mon, Aug 16, 2010 at 3:54 PM, asad azmi <azmiasadayub@gmail.com> wrote:
dear all,
 
good day.
 
 what is the purpose of using a dual certified material.
 
 
 Example -  Plate  used for vessel fabrication as per ASME SEC VIII DIV1 is  dual certified as SA 516 GR 60 and SA 516GR70.
 
What will be the tensile strength of this plate and impact properties. whether these properties will be as per SA516 GR 60  OR sa 516 GR. 70.
 
Thanks in Advance.
 
Regards
 
Asad

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...