Can anyone suggest what is the significance of ferrit count? What does manufacturer or user get from it, I mean if FC is 48%, whats it gona cause and what prevent?
-- On Tue, Aug 17, 2010 at 8:23 AM, Yoon <ych93@hotmail.com> wrote:
above value mentioned by Mr Bathula is for weld metal, not base
meterial.
Regards
On Aug 17, 2:02 pm, "Bathula Raghuram (Mumbai - PIPING)"
<R.Bath...@ticb.com> wrote:> Filtered by Hosted Filtering- Hide quoted text -
> For Duplex SS it would be 30-60% and austenitic SS 3-10% (except 310)
>
>
>
> -----Original Message-----
> From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Yoon
> Sent: Tuesday, August 17, 2010 10:16 AM
> To: Materials & Welding
> Subject: [MW:6533] Re: value of ferrite content
>
> The chemical analysis of S31803 is designed to obtain 50% ferrite contents.
> The range of ferrite content depends on actual chemical contents.
>
> I think carbon content for C.S or S.S is not important. Anyway ferritic carbon steel : approxi. 100%, austenitic stainless steel:
> approxi. 0%.
>
> Regards,
>
> On Aug 17, 10:38 am, skrie85 <skri...@yahoo.com> wrote:
> > What the range value/percentage for ferrite content of duplex (SA240
> > UNS 31803) , Stainless steel and Carbon steel?
>
>
> - Show quoted text -
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment